Many coating defects form at the surface while the film is still wet: craters around contaminants, Bénard cells as solvent evaporates, colour floating and flooding, poor spreading on low-energy substrates, and films that block or feel rough once dry. Polyether-modified silicone additives work at that surface by lowering and evening out surface tension.
Silfluo offers two groups. Silicone leveling agents handle flow, crater control, slip, anti-blocking and recoatability in organic coatings. Substrate wetting agents help waterborne industrial coatings spread over difficult substrates. The right grade depends on the defect, the resin system and whether the coating is waterborne or solvent-borne.
The TDS for these additives covers composition, viscosity and function only, so this page helps you decide which grades to trial; addition level and compatibility come from your own tests.
Service Conditions Covered
| Coating types | Organic resin coatings (leveling agents) · waterborne industrial coatings (substrate wetting agents) |
| Defects addressed | Cratering, Bénard cells, pigment floating and flooding, poor substrate wetting, low slip, blocking, recoat problems |
| Viscosity range | 20–50 cSt (LF-2502) to 2000–3000 cSt (LF-1442) |
| Extra properties | Low foam (LF-1443, LF-2505) · acid and alkali resistance (LF-1444, LF-2505) · broad or wide pH (LF-2502, LF-2506) · clear liquid (LF-2504) · reactive (LF-1221) |
| Supply | 12 months shelf life unopened at room temperature; shipped as non-dangerous goods |
Recommended Products & Why
| Grade | Viscosity (25 °C) | Key Function | Why this grade |
|---|---|---|---|
| LF-1344 | 600–1000 cSt | Flow, leveling, anti-floating; slip | Flow and surface-defect control during drying: helps suppress Bénard cells, reduces cratering and pigment floating, and adds slip to the dried film. |
| LF-1444 | 600–1000 cSt | Leveling; recoatable; acid/alkali resistant | Leveling for recoatable systems with acid and alkali resistance; same viscosity range as LF-1344, chosen when later coats must still adhere. |
| LF-1442 | 2000–3000 cSt | Slip, anti-blocking, anti-cratering | Highest-viscosity grade at 2000–3000 cSt, aimed at surface slip and anti-blocking, with leveling and crater control as secondary effects. |
| LF-1400 | 300–500 cSt | Broad compatibility; flow and slip | Broad compatibility across resin systems for flow, smoothness and slip, for complex formulations where incompatibility is the main risk. |
| LF-1443 | 500–1000 cSt | Wetting, leveling, smooth feel; low foam | Wetting, leveling and a smooth hand feel with a low contribution to foam, for systems already prone to foaming. |
| LF-1221 | 200–500 cSt | Reactive; wetting and leveling | Reactive grade that can be built into the resin to add lubricity, softness and water repellency on top of wetting and leveling. |
| LF-2502 | 20–50 cSt | Substrate wetting; broad pH range | Low-viscosity waterborne wetting agent for low-surface-energy substrates, supporting uniform films across a broad pH range. |
| LF-2504 | 40–100 cSt | Substrate wetting and leveling; clear liquid | Clear liquid wetting agent for waterborne coatings that also supports leveling, where a clear additive is required. |
| LF-2505 | 200–300 cSt | Substrate wetting; low foam; acid/alkali resistant | Waterborne wetting with low foam and resistance to acidic or alkaline conditions; supplied as a yellow transparent liquid. |
| LF-2506 | 20–40 cSt | Wetting, leveling and slip; wide pH | Wetting, leveling and slip over a wide pH range while limiting foam stabilization, as a single additive in simpler formulations. |
Table values from each product's TDS; “—” = not listed in that TDS.
Surface Preparation & Application Principles
Identify the defect before choosing the additive. Craters and Bénard cells point to a leveling agent; retraction and poor coverage on low-energy substrates point to a wetting agent; blocking and rough feel point to a slip grade.
Add silicone additives in small steps and compare each level against an untreated control panel, checking appearance, foam and adhesion together rather than the target defect alone.
Check recoatability and intercoat adhesion whenever a silicone additive goes into a primer or intermediate coat, or start with LF-1444 where recoating is part of the system.
Trial one or two matched grades against your current additive at the same addition level, rather than several similar grades at once; side-by-side results are easier to read.
Applicability Boundaries & What We Confirm
- Dosage, VOC and certification figures are not stated in our TDS, and we do not publish them.
- Substrate wetting agents are described for waterborne industrial coatings; use in solvent-borne systems needs testing.
- Silicone additives can affect recoating and intercoat adhesion in some systems; verify adhesion before production.
- What we confirm: waterborne or solvent-borne, resin system, substrate, the defect, the additive you use now and why you want to change, and whether the trial is for development or production.
Discuss your project with an engineer
Send your substrate, service conditions and current coating problem — we reply with a concrete system proposal within 1 business day.